FORMATION OF OPTIMAL TAPER FOR DIRECTIONAL CASTING SOLIDIFICATION
https://doi.org/10.17073/0368-0797-2014-12-39-41
Abstract
In this paper a method of calculating the optimum power cone of wall castings was proposed up to 300 mm. The experimental test data of calculated taper equation was presented. It was shown that the use of rainwater gating system at a negative taper allows creating conditions for the withdrawal of shrinkage cavity in profit.
About the Author
V. P. AntonovRussian Federation
Cand.Sci. (Eng.),Assist. Professor
References
1. Vishnyakov A.V., Mikhailets S.N. Proizvodstvo stali i ferosplavov. Trudy Sibirskogo metallurgicheskogo instituta [Production of steel and ferroalloys. Proceedings of the Siberian Metallurgical Institute]. Issue 6. Novokuznetsk: izd. SMI, 1969. 199 p. (In Russ.).
2. Gulyaev B.B. Zatverdevanie i neodnorodnost’ stali [Solidification and heterogeneity of steel]. Moscow – Leningrad: Metallurgizdat, 1950. 227 p. (In Russ.).
3. Nehendzi Yu.A. Stal’noe lit’e [Steel casting]. Moscow: Metallurgizdat, 1949. 707 p. (In Russ.).
4. Vasilevskiy P.F. Tehnologiya stal’nogo lit’ya[Steel casting technology]. Moscow: Mashinostroenie, 1974. 408 p. (In Russ.).
5. Antonov V.P., Taran N.I., Klimov V.Ya., Shvidkov N.I. The method of calculating the metal cooling during the filling of the mold through an intermediate device with a gating system. Liteishchik Rossii. 2012, no.10, pp. 37–40. (In Russ.).
6.
Review
For citations:
Antonov V.P. FORMATION OF OPTIMAL TAPER FOR DIRECTIONAL CASTING SOLIDIFICATION. Izvestiya. Ferrous Metallurgy. 2014;57(12):39-41. (In Russ.) https://doi.org/10.17073/0368-0797-2014-12-39-41