BASIS OF DESIGN OF A HIGH-TEMPERATURE ABRASIVE WEAR OF A ROTARY CRUSHER OF AGGLOMERATE
https://doi.org/10.17073/0368-0797-2013-12-23-27
Abstract
The main factor of a high-temperature abrasive wear of a rotary crusher is the geometrical one, which is characterized by the depth of penetration ratio hв to the radius of an abrasive particle ra , i.e. hв / ra. The second factor is the physical-mechanical one, which is characterized by the ratio of tangential strength of molecular bond τa to the material yield point σт , i.e., τa / σт . For the support of an abrasive wear without microcutting the sum of the ratio has to satisfy the following condition hв / ra + τa / σт ≤ 0,5.
About the Author
V. A. BystrovRussian Federation
References
1. Энциклопедический словарь по металлургии. Т. 1 / Под ред. Н.П. Лякишева. – М.: Интернет Инжиниринг , 2000. – 468 с.
2. Вегман Е.Ф. Краткий справочник доменщика. – М.: Металлургия, 1981. – 240 с.
3. Тененбаум М.М. Сопротивление абразивному изнашиванию. – М.: Машиностроение, 1976. – 271 с.
4. Пилюшенко В.Л., Шаповалов Ю.С. // Изв. вуз. Черная металлургия. 1991. № 6. С. 108, 109.
5. Быстров В.А., Борискин И.К., Верёвкин В.И. // Изв. вуз. Черная металлургия. 1994. № 4. С. 6 – 9.
6. Шехтер С.Я., Пьянков В.В. – В кн.: Наплавка. Опыт и эффективность применения. – Киев: изд. ИЭС им. Е.О. Патона, 1985. С. 3 – 9.
7. Быстров В.А., Новиков Н.И., Лубяной Д.А. Экономическая эффективность инноваций, направленных на повышение долговечности сменного металлургического оборудования // Современное предпринимательство: монография / Под общ. ред. О.И. Кирикова. Кн. 18. – Воронеж: изд. ВГПУ, 2007. – 320 с.
Review
For citations:
Bystrov V.A. BASIS OF DESIGN OF A HIGH-TEMPERATURE ABRASIVE WEAR OF A ROTARY CRUSHER OF AGGLOMERATE. Izvestiya. Ferrous Metallurgy. 2013;56(12):23-27. (In Russ.) https://doi.org/10.17073/0368-0797-2013-12-23-27