Service conditions and a high-temperature abrasive wear of rolls are observed. Principal causes of roll wear are thermal, oxidative, frictional and abrasive ones, and also thermal cracks are formed on a roll surface as a result of cyclic heating and cooling during operating process. Durability increase measures of mill rolls are shown in the paper.
About the Authors
V. A. BystrovRussian Federation
Dr. Eng., Professor
P. K. Dyakov
Russian Federation
Postgraduate
A. G, Umanets
Russian Federation
Postgraduate
References
1. Skorokhodov V.N., Chernov P.P. Stal’. 2001. № 8. Pp. 8 – 13.
2. Sinnave M., Gostev K.I. Stal’. 2001. № 8. Pp. 2 – 8.
3. Budag’yants N.A., Karsskiy V.E. Litie prokatnie valki (Cast rolls). Мoscow: Metallurgiya, 1983. 540 p.
4. Kashchenko F.D., Frumin I.I. Sovremennie sposobi naplavki (Modern methods of welding). Kiev: IES im. Е.О. Patona, 1982. Pp. 24 – 29.
5. Leshchinskiy L.K., Gulakov S.V. etc. Naplavka. Opit i effektivnost’ primeneniya (Built-up welding. Experience and effi ciency of application). Kiev: IES im. Е.О. Patona, 1985. Pp. 17 – 20.
6. Medovar L.B., Tsikulenko А.K., Shevchenko V.Е. Problemi SEM. 2001. № 1. Pp. 38 – 48.
7. Bistrov V.А., Veryovkin V.I., Selyanin I.F. Izv. vuz. Chernaya metallurgiya. 2001. № 8. Pp. 64 – 66.
8. Bistrov V.А., Veryovkin V.I., Selyanin I.F. Vestnik gorno-metallurgicheskoy Sektsii RAEN. Otdelenie metallurgii. 2005. Issue 14. Pp. 129 – 140.
9. Bistrov V.А., Veryovkin V.I. Sb. nauchn. trudov KemGU. Vip. 5 (Collected scientifi c works of KemSU. Issue 5.). Kemerovo: izd. KemGU, 2010. Pp. 343 – 348.
10.
Review
For citations:
Bystrov V.A., Dyakov P.K., Umanets A.G. OPERATING CONDITIONS AND WEAR OF HOT METAL MILL ROLLS. Izvestiya. Ferrous Metallurgy. 2014;57(5):24-29. (In Russ.) https://doi.org/10.17073/0368-0797-2014-5-24-29